Vol.13, No.3, August 2010

Effect of Preparation Parameters of Sulfur Cathodes on Electrochemical Properties of Lithium Sulfur Battery
JKES Vol.13, No.3, pp.169~174, August 2010
DOI : 10.5229/JKES.2010.13.3.169
Xiaohui Zhao, Dul-Sun Kim, Hyo-Jun Ahn, Ki-Won Kim, Chang-Soo Jin, and Jou-Hyeon Ahn
Department of Chemical and Biological Engineering and Engineering Research Institute, Gyeongsang National University, 900, Gajwa-dong, Jinju 660-701, Republic of Korea School of Materials Science and Engineering, Gyeongsang National University, 900, Gajwa
Sulfur cathodes were prepared by ball milling method with different types of electronic conductors and binders in different ball milling time. The sulfur cell with a cathode prepared in 45 min ball milling time gave an initial discharge capacity of 794mAh
Keyword : Lithium sulfur battery, Electronic conductor, Binder, Ball milling time, Cycle property

Full Text PDF 다운로드

위로가기

COPYRIGHT (C) KECS. ALL RIGHTS RESERVED.

  • 사업자등록번호: 209-82-06548
  • 사업자명: (사)한국전기화학회
  • 대표자: 이재준
  • 주소: 06132 서울시 강남구 테헤란로25길 20 역삼현대벤쳐텔 510호 (역삼동, 642-1 )
  • 대표전화: +82-2-568-9392
  • 자주하는 질문 (FAQ)
  • 전자우편: kecs98@kecs.or.kr (대표)